Electrical Properties Metric English Comments
Electrical Resistivity 0.000034 ohm-cm
0.000034 ohm-cm
Pacific Sintered Materials BZN-131-U Nickel Silver Powdered Metal
Higher strength than brass. Good corrosion resistance.Equivalent MPIF Specification: CZN-1818-17All information provided by Pacific Sintered Metals.