PSM Industries Pacific Sintered Metals Steel F-240-S Powdered Metal

Category Metal , Ferrous Metal
Manufacturer PSM Industries
Trade Name Pacific Sintered Metals
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PSM Industries Pacific Sintered Metals Steel F-240-S Powdered Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium stressed mechanical components Equivalent MPIF Specification: F-0005-25Information Provided by Pacific Sintered Metals, a division of PSM Industries
Physical Properties Metric English Comments
Density 6.80 - 7.20 g/cc
0.246 - 0.260 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 55
55
Tensile Strength, Ultimate 262 MPa
38000 psi
Tensile Strength, Yield 193 MPa
28000 psi
Elongation at Break 2.0 %
2.0 %
1 in. gauge
Tensile Modulus 124 GPa
18000 ksi
Flexural Strength 524 MPa
76000 psi
Transverse Rupture
Charpy Impact, Unnotched 6.78 J
5.00 ft-lb