Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 124 GPa | 18000 ksi | |
PSM Industries Pacific Sintered Metals Steel F-240-S Powdered Metal Medium stressed mechanical components Equivalent MPIF Specification: F-0005-25Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Modulus | 124 - 159 GPa | 18000 - 23100 ksi | |
Goodfellow Manganin® Copper Resistance Alloy Resistance alloy with moderate resistivity and low temperature coefficient. The resistance/temperature curve is not as flat as the constantans nor are the corrosion resistance properties as good.In.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 706 Copper Nickel 10%, 1/2 Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 706 Copper Nickel 10%, 1/4 Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 706 Copper Nickel 10%, Extra Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 706 Copper Nickel 10%, Spring 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 735 Nickel Silver 18%, 1/2 Hard 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 735 Nickel Silver 18%, 1/4 Hard 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 735 Nickel Silver 18%, Extra Hard 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 735 Nickel Silver 18%, Extra Spring 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 735 Nickel Silver 18%, Hard 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 735 Nickel Silver 18%, Spring 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 752 Nickel Silver 18%, 1/4 Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 752 Nickel Silver 18%, Annealed Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 752 Nickel Silver 18%, Extra Spring Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 752 Nickel Silver 18%, Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 752 Nickel Silver 18%, Spring Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 762 Nickel Silver 12%, 1/2 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 762 Nickel Silver 12%, 3/4 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 762 Nickel Silver 12%, Extra Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 762 Nickel Silver 12%, Extra Spring 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 762 Nickel Silver 12%, Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 770 Nickel Silver 18%, 1/2 Hard 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 770 Nickel Silver 18%, 3/4 Hard 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 770 Nickel Silver 18%, Extra Hard 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 770 Nickel Silver 18%, Extra Spring 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 770 Nickel Silver 18%, Hard 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 770 Nickel Silver 18%, Spring 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | Typical |
Dura-Bar G2 Continuously Cast Gray Iron Bar Stock ASTM A48 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as an alternative to gray i.. |
|||
Tensile Modulus | 124 GPa | 18000 ksi | |
Eagle Brass 752 Nickel Silver 18%, Extra Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |