Material Notes:
A high purity, fine, dry ground natural calcium carbonate.Applications: Plastic applications such as rigid PVC, flexible PVC, and polyolefins. Paint applications such as water based, solvent based, and high gloss powder coatings.Information supplied by Omya North America.
Physical Properties Metric English Comments
Specific Gravity 2.71 g/cc
2.71 g/cc
Brightness 95 %
95 %
Y - Brightness (dry)
Moisture Absorption at Equilibrium 0.070 %
0.070 %
Moisture Loss at 110°C % (dry)
Particle Size 2.0 µm
2.0 µm
Median Diameter
Descriptive Properties Value Comments
Calcium Carbonate % 97
FDA 21 CFR 174.5, 175.300, 178.3297
Hegman (dry) 6
Magnesium Carbonate % 0.5
Retained in 325 mesh (dry) ppm 0.0003