Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
Omya OMYACARB® 2 - AZ Calcium Carbonate A high purity, fine, dry ground natural calcium carbonate.Applications: Plastic applications such as rigid PVC, flexible PVC, and polyolefins. Paint applications such as water based, solvent based, .. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
Omya OMYACARB® 3 - AZ Calcium Carbonate A dry ground calcium carbonate with excellent fineness, color, and dispersion characteristics.Applications: Rubber and plastic applications such as rigid and plasticized PVC. Also used in paints, pu.. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
Omya OMYACARB® 6 - PT Calcium Carbonate A dry ground calcium carbonate with intermediate and closely sized particle distribution.Applications: An ideal extender for plastics, rubber, coating, and caulks. Designed for use in unsaturated po.. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
Omya PULPROWHITE® 10 - SA Calcium Carbonate A dry ground calcium carbonate with an intermediate and closely sized particle distribution.Information supplied by Omya North America. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
Omya PULPROWHITE® 17 - SA Calcium Carbonate A dry ground calcium carbonate with a broad particle distribution and closely controlled top size.Information supplied by Omya North America. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
Omya PULPROWHITE® 20 - SA Calcium Carbonate A dry ground calcium carbonate with a medium and closely sized particle distribution and excellent shrink resistance properties.Information supplied by Omya North America. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
Omya PULPROWHITE® 3 - SA Calcium Carbonate A dry ground calcium carbonate with excellent fineness and dispersion characteristics.Information supplied by Omya North America. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
Omya PULPROWHITE® 8 - SA Calcium Carbonate A dry ground calcium carbonate with an intermediate and closely sized particle distribution.Information supplied by Omya North America. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
Omya SNOWHITE® 12 - PT Calcium Carbonate A dry ground calcium carbonate with an intermediate and closely sized particle distribution.Applications: An ideal extender for plastics, rubber, coating, and caulks. Designed for use in unsaturated.. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
Omya SNOWHITE® 12-40 - PT Calcium Carbonate A bright white, dry screen-separated grade.Applications: Concrete matrix and mortar sand; ASTM golf bunker sand.Information supplied by Omya North America. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
Omya SNOWHITE® 17 - PT Calcium Carbonate A dry ground calcium carbonate with an intermediate particle distribution, unique size, color, and purity.Applications: Ideal for cementitious grouts, plasters, and automotive underspray application.. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
Omya SNOWHITE® 21 - PT Calcium Carbonate A dry ground calcium carbonate with a medium and closely sized particle distribution and excellent shrink resistance properties.Applications: Ideal for joint compounds, unsaturated polyester, cement.. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
Omya SNOWHITE® 3 - PT Calcium Carbonate A dry ground calcium carbonate with excellent fineness, color, and dispersion characteristics.Applications: Employed in rubber and plastic applications such as rigid PVC and plasticized PVC. Also us.. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
Omya SNOWHITE® 350 - PT Calcium Carbonate A dry ground, high whiteness calcium carbonate with tightly controlled top size.Applications: Aggregate for stucco and swimming pool plaster.Information supplied by Omya North America. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
Epoxy Technology EPO-TEK® E3001-6 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E3001-HV is a snap cure, single component, silver-filled die attach adhesive for semiconductor plastic IC packaging. Also available in a frozen syringe. Advantages & .. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
CIMBAR RiverCal™ 8107 & 8107C Calcium Carbonate (CaCO3) RiverCal™ 8100 Series Calcium Carbonate are high purity, white, functional fillers targeted for use in thermosets, thermoplastics, paint & coatings, sealants, TPO's and TPE's and other applications.. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
CIMBAR RiverCal™ 8103 & 8103C Calcium Carbonate (CaCO3) RiverCal™ 8100 Series Calcium Carbonate are high purity, white, functional fillers targeted for use in thermosets, thermoplastics, paint & coatings, sealants, TPO's and TPE's and other applications.. |
|||
Specific Gravity | 2.71 g/cc | 2.71 g/cc | |
CIMBAR RiverCal™ 8105 & 8105C Calcium Carbonate (CaCO3) RiverCal™ 8100 Series Calcium Carbonate are high purity, white, functional fillers targeted for use in thermosets, thermoplastics, paint & coatings, sealants, TPO's and TPE's and other applications.. |