Nye Lubricants UniFlor 8120 (473) (UF) Synthetic Oil

Category Fluid , Lubricant , Perfluoropolyether (PFPE)
Manufacturer Nye Lubricants
Trade Name UniFlor
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants UniFlor 8120 (473) (UF) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 96
96
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 31 cSt
31 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
Base Oil; ASTM D445
Evaporation Loss 6.0 %
6.0 %
24 hrs, 150C; ASTM D972
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Recommended
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Recommended
Pour Point -54.0 °C
-65.2 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type PFPE(pnd)