Nye Lubricants 609 (SO) Synthetic Oil

Category Fluid , Lubricant , Synthetic Ether Base
Manufacturer Nye Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants 609 (SO) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 61
61
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 39 cSt
39 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 5.5 cSt
5.5 cSt
Base Oil; ASTM D445
Evaporation Loss 9.0 %
9.0 %
6.5 hrs, 204C; ASTM D972
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Recommended
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Recommended
Pour Point -43.0 °C
-45.4 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type Ester(Di)