Material Notes:
Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applications replacing talc-filled, glass-filled or virgin polypropylene.Information provided by Noble Polymers.
Physical Properties Metric English Comments
Specific Gravity 0.928 g/cc
0.928 g/cc
ASTM D792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Melt Flow 30.2 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30.2 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.10 MPa
3785 psi
ASTM D638
Elongation at Break 16.8 %
16.8 %
ASTM D638
Izod Impact, Notched 0.587 J/cm

@Temperature 23.0 °C
1.10 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Tangent Modulus 1660 MPa
241000 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 114.0 °C
237.2 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 58.00 °C
136.4 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature