Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.928 g/cc | 0.928 g/cc | ASTM D792 |
PolyOne Maxxam™ FR PP 401 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Specific Gravity | 0.928 g/cc | 0.928 g/cc | ASTM D792 |
PolyOne Maxxam™ FR PP FR 7A11 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Specific Gravity | 0.928 g/cc | 0.928 g/cc | ASTM D792 |
PolyOne Maxxam™ FR PP FR 7B01 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Specific Gravity | 0.928 g/cc | 0.928 g/cc | ASTM D792 |
PolyOne Maxxam™ FR PP FR 7B31 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Specific Gravity | 0.928 g/cc | 0.928 g/cc | ASTM D792 |
PolyOne Maxxam™ FR PP FR 7C11 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Specific Gravity | 0.928 g/cc | 0.928 g/cc | ASTM D792 |
PolyOne Versaflex™ OM 1060X-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 1060X-1 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, ABS, PC/ABSColor conce.. |
|||
Specific Gravity | 0.928 g/cc | 0.928 g/cc | ASTM D792 |
PolyOne Versaflex™ OM 1060X-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 1060X-9 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Excellent Bond to PC, ABS, PC/ABS - Good Surface Aesthetics - Rubbery Feel - Soft TouchPurge thoro.. |
|||
Specific Gravity | 0.928 g/cc | 0.928 g/cc | ASTM D792 |
PolyOne Versaflex™ OM 9-802CL Thermoplastic Elastomer (TPE) Versaflex™ OM 9-802CL is a clear, soft touch TPE designed to bond to the following thermoplastics: PC, ABS, PC/ABS and copolyester. New Product. Commercial specifications have not been established... |
|||
Specific Gravity | 0.928 g/cc | 0.928 g/cc | ISO 1183 |
Polimeri Europa Riblene® FC 40 Low Density Polyethylene - Blown Film Extrusion Riblene FC 40 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 40 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Specific Gravity | 0.928 g/cc | 0.928 g/cc | ASTM D792 |
Noble Polymers Forte™ 18CPP091 Nanocomposite Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica.. |
|||
Specific Gravity | 0.928 g/cc | 0.928 g/cc | ASTM D792 |
Noble Polymers Forte™ 35CP091 Nanocomposite Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica.. |
|||
Specific Gravity | 0.928 g/cc | 0.928 g/cc | ASTM D792 |
PolyOne Elastamax™ HTE 1104 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |
|||
Specific Gravity | 0.928 - 0.932 g/cc | 0.928 - 0.932 g/cc | ASTM D1505 |
LG Chemical SEETEC EF321 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties. Good Optical Properties. Additives : No Additive Applications: Agricultural FilmCSA No. 25895-47-0Information provided by LG Chemical |
|||
Specific Gravity | 0.928 - 0.932 g/cc | 0.928 - 0.932 g/cc | ASTM D1505 |
LG Chemical SEETEC EF443 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCSA No. 24937-78-8Information provided by LG Chemical |
|||
Specific Gravity | 0.928 g/cc | 0.928 g/cc | ASTM D792 |
E-Polymers EFLEX® V1080 EPDM/TPV V-series (Thermoplastic Vulcanizate Resins): E-FLEX V series resins are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic eq.. |
|||
Specific Gravity | 0.928 g/cc | 0.928 g/cc | ASTM D792 |
E-Polymers EFLEX® V1090 EPDM/TPV V-series (Thermoplastic Vulcanizate Resins): E-FLEX V series resins are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic eq.. |
|||
Specific Gravity | 0.928 g/cc | 0.928 g/cc | ASTM D792 |
E-Polymers EFLEX® V1140 EPDM/TPV V-series (Thermoplastic Vulcanizate Resins): E-FLEX V series resins are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic eq.. |
|||
Specific Gravity | 0.928 g/cc | 0.928 g/cc | ASTM D792 |
E-Polymers EFLEX® V1150 EPDM/TPV V-series (Thermoplastic Vulcanizate Resins): E-FLEX V series resins are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic eq.. |