NAPCO Silicon Carbide 200F, 90% SiC

Category Ceramic , Carbide
Manufacturer NAPCO
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NAPCO Silicon Carbide 200F, 90% SiC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Oxidation resistant up to about 1650°C (3000°F), high thermal conductivity, low CTE, low thermal shock, high abrasion and wear resistance, good chemical resistance. Data provided by the manufacturer, North American Processing Company.
Component Elements Properties Metric English Comments
Free C 0.00 %
0.00 %
SiC 89.8 %
89.8 %
Total C 31 %
31 %