Teknor Apex Beetle® MDM54 Nylon 6, Non-halogenated, Mineral Reinforced

Category
Manufacturer Teknor Apex Company
Trade Name Beetle®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Beetle® MDM54 Nylon 6, Non-halogenated, Mineral Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: MDM54 is a UL recognized, V-2 rated halogen and phosphorus-free flam retarded, mineral filled injection molding grade of nylon 6, primarily intended for electrical applications; U.L. 94 V-2 at 1.5mm, 960°C glow wire Features: Flame Retardant; Halogen Free; Low (to no) Phosphorus; Good ColorabilityProcessing Method: Injection molding Forms: Pellets Injection Notes: No drying is necessary unless the material has been exposed to air for longer than 3 hours; Back Pressure: Low; Injection Pressure: High; Injection Rate: FastInformation Provided by Teknor Apex
Thermal Properties Metric English Comments
Flammability, UL94 V-2

@Thickness 1.50 mm
V-2

@Thickness 0.0591 in
Processing Properties Metric English Comments
Rear Barrel Temperature 240 - 260 °C
464 - 500 °F
Middle Barrel Temperature 240 - 260 °C
464 - 500 °F
Front Barrel Temperature 240 - 260 °C
464 - 500 °F
Melt Temperature <= 300 °C
<= 572 °F
Processing Temperature
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2 hour
2 hour
Screw Speed 50 - 200 rpm
50 - 200 rpm