The burn rate is 0.53 in/min; ASTM FM VSS 302.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955-89
Melt Flow 2.8 g/10 min
2.8 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 46
46
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 12.8 MPa
1860 psi
ASTM D638-95
Elongation at Break 650 %
650 %
ASTM D638-95
Elongation at Yield 22 %
22 %
ASTM D638-95
Flexural Modulus 0.342 GPa
49.6 ksi
ASTM D790-95
Izod Impact, Notched NB
NB
ASTM D-256-93a
Tear Strength 99.5 kN/m
568 pli
ASTM D624-95