Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® A 4541 Clear TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® A 4541 Clear TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Method:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.892 g/cc
0.892 g/cc
ASTM 792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Melt Flow 96 g/10 min

@Load 2.16 kg,
Temperature 230 °C
96 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
10 seconds; ASTM D2240
Tensile Strength, Yield 2.95 MPa
428 psi
Elastic; ASTM D412
Elongation at Break 610 %
610 %
Elastic; ASTM D412
Tear Strength 21.0 kN/m
120 pli
ASTM D624
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Users viewing this material also viewed the following: