Material Notes:
Applications: Lead-free NVIS Intruder Green A filter glass for Nichia White LED sources.Information provided by Mo-Sci Corporation.
Physical Properties Metric English Comments
Density 3.20 g/cc
0.116 lb/in³
Thickness 1000 microns
39.4 mil
Thermal Properties Metric English Comments
CTE, linear 12.0 µm/m-°C
6.67 µin/in-°F
Transformation Temperature, Tg 398 °C
748 °F
Softening Point 427 °C
801 °F
Dilatometric
Optical Properties Metric English Comments
Refractive Index 1.60
1.60
Transmission, Visible 14.2 %
14.2 %
Photopic, Source NSCW100
14.8 %
14.8 %
Photopic, Source NSCW455
UV Transmittance 0.00 %

@Wavelength 430 nm
0.00 %

@Wavelength 430 nm
0.010 %

@Wavelength 390 nm
0.010 %

@Wavelength 390 nm
0.10 %

@Wavelength 480 nm
0.10 %

@Wavelength 480 nm
0.30 %

@Wavelength 530 nm
0.30 %

@Wavelength 530 nm
0.50 %

@Wavelength 580 nm
0.50 %

@Wavelength 580 nm
Descriptive Properties Value Comments
Chromaticity, CIE 1976 0.1
u', Source NSCW455
0.1
u', Source NSCW100
0.55
v', Source NSCW100
0.55
v', Source NSCW455
NVIS Radiance 4.1E-12
NR(b), MIL-STD-3009@0.1 fL Luminance, Source NSCW455
4.2E-12
NR(b), MIL-STD-3009@0.1 fL Luminance,, Source NSCW100
5.4E-11
NR(a), MIL-STD-3009@0.1 fL Luminance, Source NSCW455
5.5E-11
NR(a), MIL-STD-3009@0.1 fL Luminance, Source NSCW100
Tolerance Radius 0.01
r', Source NSCW007
0.01
r', Source NSCW100
0.01
r', Source NSCW455