Möller Medical TafSkin 109 L NanoCoating

Category Ceramic , Glass , Glass Ceramic , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Moeller Medical (Möller Medical)
Trade Name TafSkin
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Möller Medical TafSkin 109 L NanoCoating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Electrically conducting, chemical-resistant, thin, easy-to-clean PTFE coatingInformation provided by Möller Medical, Member of CENTROTEC Group
Physical Properties Metric English Comments
Thickness 2.00 - 10.0 microns
0.0787 - 0.394 mil
Mechanical Properties Metric English Comments
Taber Abrasion, mg/1000 Cycles 30
30
CS17 friction disc with 500g load; DIN 53754
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Processing Properties Metric English Comments
Processing Temperature 340 - 400 °C
644 - 752 °F
Hardening Temperature
Descriptive Properties Value Comments
Applicable Substrate Aluminum
Copper
Glass
with restrictions
Stainless Steel
Biocompatibility Biocompatible
One-parametric cytotoxicity test
Contact Angle to Water [deg] 109
Cupping Test [mm] 5.2
DIN EN ISO 1520
Non-Applicable Substrate ABS
Brass
Nylon
PMMA
Polycarbonate
Tubes int. dia. 0.1-10 mm
Pendulum Dampening Test [sec] 140-150
DIN EN ISO 1522