MetalTek MTEK CW-2M Cast UNS N26455 Severe Corrosion and Heat Resistant Alloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer MetalTek
Trade Name MTEK
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK CW-2M Cast UNS N26455 Severe Corrosion and Heat Resistant Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MetalTek
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 495 MPa
>= 71800 psi
Tensile Strength, Yield >= 275 MPa
>= 39900 psi
Elongation at Break >= 20 %
>= 20 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.020 %
<= 0.020 %
Chromium, Cr 15 - 17.5 %
15 - 17.5 %
Iron, Fe <= 2.0 %
<= 2.0 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo 15 - 17.5 %
15 - 17.5 %
Nickel, Ni 60.18 - 70 %
60.18 - 70 %
As Balance
Silicon, Si <= 0.80 %
<= 0.80 %
Tungsten, W <= 1.0 %
<= 1.0 %
Descriptive Properties Value Comments
Heat Treatment Sol. Anneal