Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 495 MPa

@Temperature 500 °C
71800 psi

@Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 253MA® High Temperature Austenitic Stainless Steel
Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be..
Tensile Strength, Ultimate 495 MPa
71800 psi
Kennametal Stellite Denertiaâ„¢ N8 Nickel Dental Alloy
Denertiaâ„¢ N8 is a low-carbon nickel based porcelain-bonding alloy for the manufacture of dental crowns and bridges.This alloy is Beryllium and Cadmium free as defined by ISO 22674Information pr..
Tensile Strength, Ultimate >= 495 MPa
>= 71800 psi
MetalTek HASTELLOY® S Severe Corrosion and Heat Resistant Alloy
Information provided by MetalTek
Tensile Strength, Ultimate >= 495 MPa
>= 71800 psi
MetalTek MTEK CW-12MW Cast UNS N30002 Severe Corrosion and Heat Resistant Alloy
Information provided by MetalTek
Tensile Strength, Ultimate >= 495 MPa
>= 71800 psi
MetalTek MTEK CW-2M Cast UNS N26455 Severe Corrosion and Heat Resistant Alloy
Information provided by MetalTek