MetalTek MTEK 65+Ni UNS C91600 Gear Bronze

Category Metal , Nonferrous Metal , Copper Alloy , Bronze
Manufacturer MetalTek
Trade Name MTEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK 65+Ni UNS C91600 Gear Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Copper-tin alloy with high tensile, yield and compressive strength as well as wear resistance.Applications: Worm gears, steel mill nutsInformation provided by MetalTekCast UNS C91600; Cast Grade C91600; Cast ASTM B427 ; Military MIL-C-15345-23
Mechanical Properties Metric English Comments
Hardness, Brinell 106
106
500 kg
Tensile Strength, Ultimate >= 310 MPa
>= 45000 psi
Tensile Strength, Yield >= 170 MPa
>= 24700 psi
Elongation at Break >= 10 %
>= 10 %
Component Elements Properties Metric English Comments
Copper, Cu 88 %
88 %
Nickel, Ni 1.5 %
1.5 %
Phosphorous, P 0.20 %
0.20 %
Tin, Sn 10.5 %
10.5 %