MetalTek MTEK 316L Cast UNS J92800 Austenitic Stainless Steel

Category Metal , Ferrous Metal , Austenitic , Stainless Steel , Cast Stainless Steel , T 300 Series Stainless Steel
Manufacturer MetalTek
Trade Name MTEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK 316L Cast UNS J92800 Austenitic Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
"300" series, general corrosion resistant alloyApplications: Nuclear, chemical and food processing. Valve and pump trim.Information provided by MetalTek
Mechanical Properties Metric English Comments
Hardness, Brinell 179
179
Tensile Strength, Ultimate >= 485 MPa
>= 70300 psi
Tensile Strength, Yield >= 205 MPa
>= 29700 psi
Elongation at Break >= 30 %
>= 30 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 17 - 21 %
17 - 21 %
Iron, Fe 59.97 - 72 %
59.97 - 72 %
As Balance
Manganese, Mn <= 1.5 %
<= 1.5 %
Molybdenum, Mo 2.0 - 3.0 %
2.0 - 3.0 %
Nickel, Ni 9.0 - 13 %
9.0 - 13 %
Silicon, Si <= 1.5 %
<= 1.5 %
Descriptive Properties Value Comments
Heat Treatment Sol. Anneal