Material Notes:
WESTLAKE polyethylene EF403 is a fractional melt low-density formulation suggested for use in clarity shrink applications. This LDPE formula exhibits excellent skrinkability, and has very good optical properties.Application/UsesMedium duty produce bagsGood clarity shrink filmBags for textile itemsBeverage/Bottle overwrapFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Thickness 31.8 microns
1.25 mil
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 500 %
500 %
ASTM D882
Film Elongation at Break, TD 700 %
700 %
ASTM D882
Dart Drop 4.92 g/micron
125 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
Film Tensile Strength at Break, TD 23.4 MPa
3400 psi
ASTM D882
1% Secant Modulus, MD 179 MPa
26000 psi
ASTM D882
1% Secant Modulus, TD 221 MPa
32000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 4.0 %
4.0 %
ASTM D1003
Gloss 75 %
75 %
at 45º; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 182 - 199 °C
360 - 390 °F
with BUR of 1.5:1 or higher
Blow-up Ratio (BUR) 2.5
2.5
Descriptive Properties Value Comments
Process Film
Region US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved