Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Materion Beryllium Copper Alloy 10 Wire; HT (TH04) Temper; 1.3-12.7 mm Diameter (UNS C17500)

Category Metal , Nonferrous Metal , Beryllium Alloy , Copper Alloy
Manufacturer Materion Corporation (former Brush Wellman)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Materion Beryllium Copper Alloy 10 Wire; HT (TH04) Temper; 1.3-12.7 mm Diameter (UNS C17500).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Treatment required for max strength: 2 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Physical Properties Metric English Comments
Density 8.83 g/cc
0.319 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 750 - 970 MPa
109000 - 141000 psi
Tensile Strength, Yield 650 - 870 MPa
94300 - 126000 psi
Elongation at Break >= 10 %
>= 10 %
Modulus of Elasticity 138 GPa
20000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 200 °C
10.0 µin/in-°F

@Temperature 68.0 - 392 °F
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
Melting Point 1010 - 1050 °C
1850 - 1920 °F
Solidus 1010 °C
1850 °F
Liquidus 1050 °C
1920 °F
Component Elements Properties Metric English Comments
Beryllium, Be 0.40 - 0.70 %
0.40 - 0.70 %
Cobalt, Co 2.4 - 2.7 %
2.4 - 2.7 %
Copper, Cu 97 %
97 %
as balance
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000290 - 0.00000360 ohm-cm
0.00000290 - 0.00000360 ohm-cm
48-60% IACS Conductivity
Users viewing this material also viewed the following: