Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000290 - 0.00000360 ohm-cm | 0.00000290 - 0.00000360 ohm-cm | 48-60% IACS Conductivity |
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; HT (TH04) Temper; up to 76 mm Thickness (UNS C17500) Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Electrical Resistivity | 0.00000290 - 0.00000360 ohm-cm | 0.00000290 - 0.00000360 ohm-cm | 48-60% IACS Conductivity |
Materion Beryllium Copper Alloy 10 Rod and Bar; HT (TH04) Temper; up to 76 mm (UNS C17500) Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Electrical Resistivity | 0.00000290 - 0.00000360 ohm-cm | 0.00000290 - 0.00000360 ohm-cm | 48-60% IACS Conductivity |
Materion Beryllium Copper Alloy 10 Wire; HT (TH04) Temper; 1.3-12.7 mm Diameter (UNS C17500) Treatment required for max strength: 2 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Electrical Resistivity | 0.00000290 - 0.00000360 ohm-cm | 0.00000290 - 0.00000360 ohm-cm | 48-60% IACS Conductivity |
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; HT (TH04) Temper; up to 76 mm Thickness (UNS C17510) Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Electrical Resistivity | 0.00000290 - 0.00000360 ohm-cm | 0.00000290 - 0.00000360 ohm-cm | 48-60% IACS Conductivity |
Materion Beryllium Copper Alloy 3 Rod and Bar; HT (TH04) Temper; up to 76 mm (UNS C17510) Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Electrical Resistivity | 0.00000290 - 0.00000360 ohm-cm | 0.00000290 - 0.00000360 ohm-cm | 48-60% IACS Conductivity |
Materion Beryllium Copper Alloy 3 Tube; HT (TH04) Temper; up to 76 mm o.d. (UNS C17510) Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc... |
|||
Electrical Resistivity | 0.00000290 - 0.00000360 ohm-cm | 0.00000290 - 0.00000360 ohm-cm | 48-60% IACS Conductivity |
Materion Beryllium Copper Alloy 3 Wire; HT (TH04) Temper; 1.3-12.7 mm Diameter (UNS C17510) Treatment required for max strength: 2 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials .. |
|||
Electrical Resistivity | 0.00000290 - 0.00000360 ohm-cm | 0.00000290 - 0.00000360 ohm-cm | 48-60% IACS Conductivity |
Materion Beryllium Copper Alloy 3 Strip; HT (TH04) Temper (UNS C17510) Treatment required for max strength: 2-3 hrs @ 480ºC or Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 75%Formability Ratio.. |