Mateck GaSb

Category Other Engineering Material , Semiconductor
Manufacturer Mateck GmbH
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mateck GaSb.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Semiconductor single crystals
Descriptive Properties Value Comments
Carrier Concentration (cm^-3) 1E16-5E16
Doping: Hi-R, Type: P
1E16-5E16
Doping: Hi-R, Type: N
1E18-5E18
Doping: Zn, Type: P+
2E+16
Doping: None, Type: P
2E17-6E17
Doping: Te, Type: N
EPD (cm^-2), MAX 1000
Growth Techniques Czochralski & LEC