Material Notes:
Scotch® Tape 896 is a general-purpose medium tensile strength tape reinforced with continuous glass-yarn filaments. The white backing provides an excellent “background” surface for custom-printed tape applications using “topside” flexographic printing methods and 3M™ PrintSeal™ process. The aggressive packaging-grade adhesive is specifically formulated to provide balance performance, having both high initial adhesion and long-term holding power to most fiberboard surfaces. Suitable for use in most general-purpose box closing, bundling, and pallet unitizing applications.Information provided by 3M
Physical Properties Metric English Comments
Thickness 137 microns
5.40 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 MPa
2900 psi
ASTM D3759
Elongation at Break 3.0 %
3.0 %
ASTM D3759
Peel Strength 0.657 kN/m
3.75 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Pressure sensitive synthetic rubber resin
Appearance White