MV Labs SM810 Sm2O3 Samarium oxide

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs SM810 Sm2O3 Samarium oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 348.7 g/mol
348.7 g/mol
Descriptive Properties Value Comments
Assay 86% Sm
CAS Number 12060-58-1
Form Yellow powder
Purity 99.999%
Typical Impurities Check with Manufacturer