Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 348.7 g/mol | 348.7 g/mol | |
MV Labs SM800 Sm2O3 Samarium oxide Information provided by MV Laboratories. |
|||
Molecular Weight | 348.7 g/mol | 348.7 g/mol | |
MV Labs SM810 Sm2O3 Samarium oxide Information provided by MV Laboratories. |