MV Labs CE700 Ce(NO3)3·6H2O Cerium(III) nitrate hexahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs CE700 Ce(NO3)3·6H2O Cerium(III) nitrate hexahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 434.22 g/mol
434.22 g/mol
Descriptive Properties Value Comments
Assay 32% Ce
CAS Number 10294-41-4
Form Pale yellow crystals
Purity 99.999%
Typical Impurities Rare Earths =10 ND; Ca = 7; Fe, Mg = 5 ppm