Polymer Property : Molecular Weight = 434.22 g/mol
Polymer Property :
Molecular Weight =
434.22 g/mol
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Molecular Weight
434.22
g/mol
434.22
g/mol
MV Labs CE700 Ce(NO3)3·6H2O Cerium(III) nitrate hexahydrate
Information provided by MV Laboratories.