Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M. Holland Company SA500 Styrene Acrylonitrile

Category Polymer , Thermoplastic , SAN Polymer
Manufacturer M. Holland Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company SA500 Styrene Acrylonitrile.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High clarityGood processabilityHigh stiffnessApplications: Color concentratesCompounding
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
23/23°C; ASTM D792
Melt Flow 26 g/10 min
26 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Elongation at Break 1.8 %
1.8 %
ASTM D638
Flexural Modulus 4.21 GPa
610 ksi
ASTM D790
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256
Optical Properties Metric English Comments
Haze 0.40 %
0.40 %
ASTM D1003
Transmission, Visible 94 %
94 %
ASTM D1003
Descriptive Properties Value Comments
Acrylonitrile concentration % 28-31
Forms Pellets
Processing Methods Injection molding