Material Notes:
Features: Medium Flow, High Impact Resistance, Good StiffnessUses: Appliances, Business, Equipment, Tool/Tote Box, ToysApprovals: FDA 21 CFR 177.1520 Processing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 99
99
ASTM D785
Tensile Strength, Yield 28.3 MPa
4100 psi
Type I, 2 in/min; ASTM D638
Elongation at Break 160 %
160 %
Type I, 2 in/min; ASTM D638
Flexural Modulus 1.34 GPa
195 ksi
at 0.05 in/min; ASTM D790
Izod Impact, Notched 0.961 J/cm
1.80 ft-lb/in
at 73°F; ASTM D256
Gardner Impact 28.24 J
20.83 ft-lb
0.125 in; ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C
210 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.7 °C
125 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Form Pellets