LyondellBasell Adflexâ„¢ KS311P Polyolefin

Category Polymer , Film , Thermoplastic , Polyolefin , Polyolefin, Film Grade , Polyolefin, Film Grade (Polyolefin)
Manufacturer LyondellBasell
Trade Name Adflex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Adflexâ„¢ KS311P Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Adflexâ„¢ KS-311P thermoplastic olefin resin is a barefoot formulation (no slip, no antiblock) designed for cast film extrusion applications. It is based on proprietary Basell process technology KS-311P resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.2600 for rubber articles for repeated use applications. The final item is subject to the extraction requirements in 21 CFR 177.2600. All ingredients in KS-311P resin meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Film, cast, stationary suppliesInformation provided by Basell.
Physical Properties Metric English Comments
Density 0.892 g/cc
0.0322 lb/in³
ASTM D792
Melt Flow 9.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
ASTM D2240
Tensile Strength, Yield 15.2 MPa
2200 psi
ASTM D 638
Elongation at Break 580 %
580 %
ASTM D 638
Elongation at Yield 15 %
15 %
ASTM D 638
Flexural Modulus 0.476 GPa
69.0 ksi
1% Secant, Procedure A; ASTM D790
Izod Impact, Notched NB
NB
73°F; ASTM D256