Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.892 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.892 g/cc
0.0322 lb/in³
ASTM D792
Lushan PR298 Polypropylene Copolymer Adhesive for Steel Pipe Coating
Polypropylene copolymer adhesive resin Lushan PR298 is maleic grafted polymer in granule form. It is a high tech product and was developed by Guangzhou Hot-melt Adhesive Engineering and Technical R&..
Density 0.892 g/cc
0.0322 lb/in³
ASTM D792
LyondellBasell Adflexâ„¢ KS311P Polyolefin
Description: Adflexâ„¢ KS-311P thermoplastic olefin resin is a barefoot formulation (no slip, no antiblock) designed for cast film extrusion applications. It is based on proprietary Basell proces..
Density 0.892 g/cc
0.0322 lb/in³
ASTM D792
LyondellBasell Adflexâ„¢ Q 402 F Polyolefin
Description: Adflexâ„¢ Q 402 F thermoplastic olefin resin is designed for air quenched blown film applications. Q 402 F resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 1..
Density 0.892 g/cc
0.0322 lb/in³
ASTM D792
LyondellBasell Hifaxâ„¢ CA10GC Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CA10GC fractional melt flow, 100 MPa flexural modulus, precolored, UV-stabilized, reactor grade, extrudable thermoplastic elastomeric olefin (TEO) resin combines good proces..
Density 0.892 g/cc
0.0322 lb/in³
ASTM D792
LyondellBasell Hifaxâ„¢ CA138A Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CA138A low modulus thermoplastic olefin (TPO) resin is designed for impact modification and injection molding applications. It is based on material produced from Basell'..
Density 0.892 g/cc
0.0322 lb/in³
ASTM D792
LyondellBasell Hifaxâ„¢ EP2015/60 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ EP2015/60 medium melt flow, 690 MPa flexural modulus, extrusion coating grade, specialty polypropylene copolymer has a very good balance of properties and processability. Th..
Density 0.892 g/cc

@Temperature 15.0 °C
0.0322 lb/in³

@Temperature 59.0 °F
ASTM D4052
ExxonMobil 30 Exxon XD-3
Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American d..
Density 0.892 g/cc

@Temperature 15.0 °C
0.0322 lb/in³

@Temperature 59.0 °F
ASTM D4052
ExxonMobil 30 Exxon XD-3
Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American d..
Density 0.892 g/cc
0.0322 lb/in³
ConocoPhillips Hydroclear® 320 Rock Oil
Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill ..
Density 0.892 g/cc

@Temperature 15.0 °C
0.0322 lb/in³

@Temperature 59.0 °F
ASTM D4052
ExxonMobil Mobil Delvac 40 1640
Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system.  They are specifically engineered f..
Density 0.892 g/cc

@Temperature 15.0 °C
0.0322 lb/in³

@Temperature 59.0 °F
ASTM D4052
ExxonMobil Mobil Delvac 40 1640
Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system.  They are specifically engineered f..
Density 0.892 g/cc
0.0322 lb/in³
ASTM D792
LyondellBasell Hifax™ CA207A Thermoplastic Polyolefin Elastomer
Description: Hifax™ CA207A thermoplastic olefin resin is designed to reduce shrinkage and improve paint adhesion of PP compound. It is based on proprietary Basell process technology. All ingredien..
Copyright © lookpolymers.com All Rights Reserved