Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucite International Elvacite ® 2010 Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Elvacite ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Elvacite ® 2010 Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvacite® 2010 is a medium molecular weight methyl methacrylate polymer. 2010 is excellent for use as a general purpose grade for lacquer coatings, such as barrier topcoats for vinyl. It provides high tensile strength and hardness.Applications: vinyl topcoats, general purpose grade for lacquersInformation provided by Lucite International
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Particle Size 180 - 200 µm
180 - 200 µm
Viscosity Measurement 0.383 - 0.415
0.383 - 0.415
Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 84000 g/mol
84000 g/mol
Mechanical Properties Metric English Comments
Hardness, Knoop 19
19
Tukon Hardness
Tensile Strength 72.4 MPa
10500 psi
Elongation at Break 3.5 %
3.5 %
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 98.0 °C
208 °F
Chemical Properties Metric English Comments
Total Acid Number 0.00
0.00
Processing Properties Metric English Comments
Moisture Content 0.50 %
0.50 %