Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucite International Colacryl ® TS1875 Acrylic Solution Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Colacryl ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Colacryl ® TS1875 Acrylic Solution Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Colacryl TS 1875 is a self cross-linking acrylic copolymer designed for high performance solvent resistant adhesive applications. Once dried, a film cast from this product remains permanently tacky.Suggested Uses: Pressure-sensitive self-adhesive products including high shear double-sided tapes and films which require a high degree of solvent resistance.Polyacrylate copolymerInformation provided by Lucite International
Physical Properties Metric English Comments
Solids Content 49 - 53 %
49 - 53 %
Viscosity 1500 - 7500 cP

@Temperature 25.0 °C
1500 - 7500 cP

@Temperature 77.0 °F
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Solvent Acetone N
Copyright © lookpolymers.com All Rights Reserved