Material Notes:
Description: Inherently dissipative, this patented technology delivers surface resistivity in the range of 10E8 to 10E10 O/square. Stat-Rite® IDP Polymers forms a molecular-scale, interpenetrating polymer network which carries charge. The polymeric charge carriers are permanent over time even through customer processing in injection molding or extrusion. The fundamental Estane® TPU backbone dominates in property performance. Stat-Rite® IDP (Inherently Dissipative Polymer) is a homogeneous polymer which lends itself to consistent voltage decay throughout the matrix of a finished product. Conversely alternative technologies including the use of fillers or additives can off-gas, migrate, or slough-off causing contamination at a minimum and slow or inconsistent ESD protection. Stat-Rite® IDP Elastomer Alloys are based upon TPU providing the ultimate mechanical durability, low temperature flexibility and permanent ESD protection.Major Benefits of Stat-Rite® IDP Elastomer Alloys: Permanent static dissipationUltra-cleanLow off-gassing; low ionicsClarityNo particulatesTPU performanceApplications: Clean room soft walls, windows, and doorsMaterials handling hose and tubingVacuum hose and tubingWork surface matsSpecific Notes for this Material: Newer higher electrostatic dissipation (ESD) protection, permanent ESD without carbon or anti-stats Information provided by Noveon, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength, Ultimate 26.2 MPa
3800 psi
ASTM D412/D638
Elongation at Break 450 %
450 %
ASTM D412/D638
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+9 ohm-cm
5.00e+9 ohm-cm
ASTM D257
Surface Resistivity per Square 5.00e+9 ohm
5.00e+9 ohm
ASTM D257