Electrical Properties Metric English Comments
Surface Resistivity per Square 5.00e+9 ohm
5.00e+9 ohm
50%; ASTM D257
Lubrizol STAT-RITE® S-1100 Static Dissipative TPU
Description: Stat-Rite® S1100 is a static dissipative TPU alloy. Stat-Rite S-1100 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD p..
Surface Resistivity per Square 5.00e+9 ohm
5.00e+9 ohm
ASTM D257
Lubrizol STAT-RITE® X-5091 Ether-Type Static Dissipative Polymer
Description: Inherently dissipative, this patented technology delivers surface resistivity in the range of 10E8 to 10E10 O/square. Stat-Rite® IDP Polymers forms a molecular-scale, interpenetrating ..