Lubriplate NO.3V Petroleum-Based Machine Tool Oil

Category Fluid , Lubricant
Manufacturer Lubriplate Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate NO.3V Petroleum-Based Machine Tool Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Compounded to impart a unique load carrying film, exceptional lubricity, and anti-friction properties not found in conventional oils of the same viscosity. Machine Tool Oils are available in Bottles, Jugs, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 68
68
ISO Grade
98
98
Viscosity Index
Saybolt Viscosity at 100°F 326 SUS
326 SUS
Saybolt Viscosity at 210°F 48 SUS
48 SUS
Kinematic Viscosity at 40°C (104°F) 62 cSt
62 cSt
Thermal Properties Metric English Comments
Pour Point -31.7 °C
-25.0 °F
Flammability Test 395
395
[°F] Fire Point
Flash Point 193 °C
380 °F
Descriptive Properties Value Comments
SAE Gear Oil No. 80W
SAE No. 20