Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flash Point = 193 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 193 °C
380 °F
Lubriplate APG 80W-140 Petroleum-Based Gear, Bearing, & Recirculating Oil
These heavy-duty, EP (extreme pressure) type oils were developed to meet gear oil needs of most automotive, truck, heavy equipment, and industrial gear boxes requiring an extreme pressure. Meets mil..
Flash Point 193 °C
380 °F
Lubriplate APG 80W-90 Petroleum-Based Gear, Bearing, & Recirculating Oil
These heavy-duty, EP (extreme pressure) type oils were developed to meet gear oil needs of most automotive, truck, heavy equipment, and industrial gear boxes requiring an extreme pressure. Meets mil..
Flash Point 193 °C
380 °F
Lubriplate APG-80 Petroleum-Based Gear, Bearing, & Recirculating Oil
These heavy-duty, EP (extreme pressure) type oils were developed to meet gear oil needs of most automotive, truck, heavy equipment, and industrial gear boxes requiring an extreme pressure. Meets mil..
Flash Point 193 °C
380 °F
Lubriplate SFGO Ultra-15 PAO-Based Synthetic Food Machinery Grade Fluid
Polyalphaolefin (PAO)-based high-performance fluids formulated with 100% PAO synthetic base fluids for a variety of demanding applications. They are outstanding lubricants for use under severe condi..
Flash Point 193 °C
380 °F
Heatbath/Park Vacuum Quench Oil
For use in quenching in integral vacuum furnaces. Offers excellent quenching rate and thermal stability, good viscosity, and low volatility.Information provided by Heatbath Corporation - Park Metal..
Flash Point 193 °C
380 °F
Lubriplate NO.3V Petroleum-Based Machine Tool Oil
Compounded to impart a unique load carrying film, exceptional lubricity, and anti-friction properties not found in conventional oils of the same viscosity. Machine Tool Oils are available in Bottles..
Flash Point 193 °C
379 °F
open cup
Dow Corning 702 DIFFUSION PUMP FLUID
A clear, mixed phenylmethyl dimethyl cyclosiloxane fluid designed for fast pumping of large volumes of gas down from 10-5 to 10-7. Also used on vapor ejector pumps that attain vacuums of 10-4 to 10-..
Flash Point 193 °C
379 °F
ASTM D92
ChevronTexaco Regal® N-100 R&O
Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high..
Flash Point >= 193 °C
>= 379 °F
ASTM D92
ExxonMobil Mobil Vaprotec Light
Mobil Vaprotec Light is an ISO Viscosity Grade 32, turbine-quality circulation oil containing anti-oxidants and defoamants. It is enhanced with a three-phase rust inhibitor to protect surfaces light..
Flash Point 193 °C
379 °F
ConocoPhillips MV22 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Flash Point 193 °C
379 °F
ASTM D92
ChevronTexaco Superla® 13 White Oil
FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch..
Flash Point >= 193 °C
>= 379 °F
ASTM D92
ExxonMobil Mobil Vaprotec Light
Mobil Vaprotec Light is an ISO Viscosity Grade 32, turbine-quality circulation oil containing anti-oxidants and defoamants. It is enhanced with a three-phase rust inhibitor to protect surfaces light..
Copyright © lookpolymers.com All Rights Reserved