Material Notes:
These water resistant calcium type greases are designed for plain bearings, cams, slides, and other light-duty applications where temperatures do not exceed 170°F. See special applications. Applications: Non-staining concrete form release.100 & 130 Series Greases are available in Tubes, Cans, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 300 SUS
300 SUS
Kinematic Viscosity at 40°C (104°F) 58 cSt
58 cSt
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 310
310
Unknown Amount of Work
Penetration P(60), 1/10 mm 340
340
Unknown Amount of Work
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 76.7 °C
170 °F
Minimum Service Temperature, Air -23.3 °C
-10.0 °F
Approx. Cold test
Dropping Point 82.2 °C
180 °F
ASTM Test
Descriptive Properties Value Comments
Antiwear (AW)/ Extreme Pressure (EP) AW
NLGI Grade 1
Rust/Oxidative Additives YES
Water Resistant YES