Lendell Supersoft Foams

Category Polymer , Thermoset , Polyurethane, TS
Manufacturer Lendell Manufacturing Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lendell Supersoft Foams.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Angel SkinThis line of foam has excellent feel and touch characteristics, as well as absorbency. The "breath-ability" of these foams, due to their high moisture vapor transmission qualities and the soft feel makes them ideal for skin contact applications. The foam is also formulated for use in the medical field. Applications:Outdoor Apparel, Boots, Gloves, Skin Contact Applications, Bed Comforters, Ski Goggles Lense Cleaner, Foam with Metal Dust, "New Grit" Abrasive Foam Blocks, Mattresses and PillowsInformation provided by Lendell Manufacturing Inc.
Physical Properties Metric English Comments
Density 0.0849 g/cc
0.00307 lb/in³
Water Absorption 8.5 %
8.5 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.0814 MPa
11.8 psi
ASTM D3574
Elongation at Yield 382.6 %
382.6 %
Tear Strength 0.578 kN/m
3.30 pli
Die "C", average; ASTM D3574
0.877 kN/m
5.00 pli
Average; ASTM D3574
<= 0.894 kN/m
<= 5.10 pli
Max.; ASTM D3574
Compression Set 7.3 %
7.3 %
50%; 1H%ct
16.1 %
16.1 %
50%; 1H%cd
32.4 %
32.4 %
50%; 2E%ct
35.7 %
35.7 %
50%; 1A%ct
81.4 %
81.4 %
50%; 1A%cd
87.3 %
87.3 %
50%; 2E%cd
Descriptive Properties Value Comments
CLD 50% 0.3
CLD 50% R 0.3
Comfort Factor 0.2
Expansion, % 9
in Isopropyl Alcohol
Hysteresis 17.1
IFD 25% R 5.7
ASTM D3574
IFD 25% RRT 4.7
ASTM D3574
IFD 65% 31.9
ASTM D3574
Recovery 82.9
Sag Factor 5.6
Water Retention, % 2.6
Wet Out, minutes 5