Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0849 g/cc | 0.00307 lb/in³ | |
Lendell Supersoft Foams Angel SkinThis line of foam has excellent feel and touch characteristics, as well as absorbency. The "breath-ability" of these foams, due to their high moisture vapor transmission qualities and the.. |
|||
Density | 0.0849 g/cc | 0.00307 lb/in³ | Nominal |
Hexcel® HexWeb® CR III 5/32-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Density | 0.0849 g/cc | 0.00307 lb/in³ | Nominal |
Hexcel® HexWeb® CR III 5/32-5056-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Density | 0.0849 g/cc | 0.00307 lb/in³ | Nominal |
Hexcel® HexWeb® CR-PAA™ 5/32-5052-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Density | 0.0849 g/cc | 0.00307 lb/in³ | Nominal |
Hexcel® HexWeb® CR-PAA™ 5/32-5056-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |