Kraton® G1701 E (SEP) Linear Diblock Copolymer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Kraton
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® G1701 E (SEP) Linear Diblock Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton G1701 E is a clear linear diblock copolymer based on styrene and ethylene/propylene, S-E/P, with bound styrene of 35% mass. It is supplied from Europe in the product form identified: Kraton G1701 EU - supplied as an undusted fluffy crumbRegion: Asia Pacific, Europe, Japan, North America, and South AmericaUses: Kraton G1701 E is used in formulating adhesives and coatings, as base material for compound formulations, as a modifier of thermoplastics and as base material for oil gel applications. The inherent stability of the mid block suggests the use of this grade in applications that must withstand weathering and high processing temperatures.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Packaging and Polymod; and Personal CareInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ISO 2781
Volatiles <= 0.50 %
<= 0.50 %
KM 04
Descriptive Properties Value Comments
Content Antioxidant
>0.03%, KM 08
Polystyrene
33.2-36.6%, KM 03