Kennametal Stellite Deloro® 15 Nickel Alloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Kennametal Stellite
Trade Name Deloro®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Deloro® 15 Nickel Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Deloro™ 15 is a pre-alloyed gas atomized nickel-based powder which is used primarily for the local repair of cast iron glass forming molds. It has excellent weld characteristics and is a good color match.Deloro™ 15 is typically deposited as a machinable, non-magnetic powder weld or spray-fuse (SF) deposited overlay. The fusing temperature is 1005 – 1050°C (1840 – 1920°F).Like the other Deloro™ nickel-based alloys, its wear resistance is mainly due to the presence of hard boride and silicide phases, and it retains its properties up to about 315°C (600°F). Because of its low melting point it is easily fused to form a smooth hardwearing surface.Information provided by Kennametal Stellite™
Mechanical Properties Metric English Comments
Hardness, Vickers 180 - 230
180 - 230
Thermal Properties Metric English Comments
Melting Point 1005 - 1080 °C
1841 - 1980 °F
Solidus 1005 °C
1841 °F
Liquidus 1080 °C
1980 °F
Component Elements Properties Metric English Comments
Boron, B 1.1 %
1.1 %
Carbon, C <= 0.050 %
<= 0.050 %
Copper, Cu 20 %
20 %
Iron, Fe 0.50 %
0.50 %
Nickel, Ni >= 76.35 %
>= 76.35 %
as balance
Silicon, Si 2.0 %
2.0 %
Descriptive Properties Value Comments
Application Technique Spray-fuse & powder welding