Polymer Property : Solidus = 1005 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 1005 °C
1841 °F
Kennametal Stellite Deloro® 15 Nickel Alloy
Deloroâ„¢ 15 is a pre-alloyed gas atomized nickel-based powder which is used primarily for the local repair of cast iron glass forming molds. It has excellent weld characteristics and is a good c..
Solidus 1005 °C
1841 °F
Universal Wire Works Au-Pd-Ni (AMS 4786) Gold Brazing Filler Metal
Information provided by Universal Wire Works for their line of welding wire and filler metal.
Solidus 1005 °C
1841 °F
Williams Advanced Alloys Wambraze™ WB1037 Solder
High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de..