Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Karina Karintox ENCH./03 Polyolefin Compound

Category Polymer , Thermoplastic , Polyolefin , Polyolefin, Wire/Cable Grade
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name Karintox
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina Karintox ENCH./03 Polyolefin Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Karintox is a thermoplastic polyolefin, flame retardant, non-halogen, and low smoke emission. Recommended for electrical coating for cables until 1KV. For a better usage/processing, a pre-warm/heat (2 hours in 70-80°C) is suggested, mainly after being stocked for a long time. Low compression screws (1.2:1 is the ideal) and cleaving. Thermical profile from 140ºC to 165°C and melting temperatures no more than 180°C.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.52 - 1.56 g/cc
1.52 - 1.56 g/cc
ASTM D 792
Moisture Absorption <= 0.0600 %
<= 0.0600 %
ME-53
Mechanical Properties Metric English Comments
Hardness, Shore A 93 - 97

@Time 15.0 sec
93 - 97

@Time 0.00417 hour
ASTM D 2240
Thermal Properties Metric English Comments
Oxygen Index >= 36 %
>= 36 %
ASTM D 2863
Component Elements Properties Metric English Comments
Cadmium, Cd <= 0.0050 %
<= 0.0050 %
IEC 62321
Chromium, Cr <= 0.010 %
<= 0.010 %
IEC 62321
Lead, Pb <= 0.010 %
<= 0.010 %
IEC 62321
Mercury, Hg <= 0.010 %
<= 0.010 %
IEC 62321
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
ASTM D 257
Descriptive Properties Value Comments
Application 70 Grades
Bromine, Br (%) < 0.01
IEC 62321
Users viewing this material also viewed the following: