Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Karina E 02/349-RG-GE Yellow Color Concentrate for PVC

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 02/349-RG-GE Yellow Color Concentrate for PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Color concentrate recommended for application in rigid PVC compounds for general purposes. Important Considerations:Heavy metal freeFormulated with organic and inorganic pigments PVC resin based (carrier polymer) Supplied in pellet form and packaged in 25 KG bags Recommended use of 2% to 4%Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.37 - 1.43 g/cc
1.37 - 1.43 g/cc
ASTM D 792
ASTM Color 12 - 15
12 - 15
Color A, ME 12
45.9 - 48.9
45.9 - 48.9
Color B, ME 12
59.68 - 62.68
59.68 - 62.68
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Descriptive Properties Value Comments
Application Extrusion
Injection
Pantone Classification (Natural Base) 468.00C
Users viewing this material also viewed the following: