Karina 920-10/156-Y-IS-BZ White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 920-10/156-Y-IS-BZ White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.22 - 1.28 g/cc
1.22 - 1.28 g/cc
ASTM D 792
Melt Flow 3.0 - 10 g/10 min
3.0 - 10 g/10 min
ASTM D 1238
ASTM Color -0.110 - 1.49
-0.110 - 1.49
Color A, ME 12
6.29 - 7.89
6.29 - 7.89
Color B, ME 12
90.04 - 91.64
90.04 - 91.64
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 90 - 94

@Time 15.0 sec
90 - 94

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 6.86 MPa
>= 996 psi
ASTM D 638
Elongation at Break >= 160 %
>= 160 %
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Hoses