Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.46 - 1.52 g/cc
1.46 - 1.52 g/cc
NBR NM-IEC 60811-1-3
ASTM Color -3.40 - -0.400
-3.40 - -0.400
Color B, ME 12
-1.74 - 1.26
-1.74 - 1.26
Color A, ME 12
61.94 - 64.94
61.94 - 64.94
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 86 - 90

@Time 15.0 sec
86 - 90

@Time 0.00417 hour
NBR 7456
Tensile Strength >= 12.6 MPa
>= 1820 psi
NBR NM-IEC 60811-1-1
>= 12.6 MPa
>= 1820 psi
After 168 H in Air Oven at 100°C; NBR NM-IEC 60811-1-2
Elongation at Break >= 150 %
>= 150 %
NBR NM-IEC 60811-1-1
>= 150 %
>= 150 %
After 168H in Air Oven at 100°C; NBR NM-IEC 60811-1-2
Thermal Properties Metric English Comments
Oxygen Index >= 30 %
>= 30 %
NBR 6245
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
NBR 5403
Descriptive Properties Value Comments
Application CI/CCI
Maximum Variation of Elongation (%) 25
NBR NM-IEC 60811-1-2
Maximum Variation of Tensile Strength (%) 25
NBR NM-IEC 60811-1-2