Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.21 - 1.25 g/cc
1.21 - 1.25 g/cc
ASTM D 792
ASTM Color -1.33 - 0.27
-1.33 - 0.27
Color B, ME 12
-0.850 - 0.75
-0.850 - 0.75
Color A, ME 12
24.99 - 26.59
24.99 - 26.59
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 63 - 67

@Time 15.0 sec
63 - 67

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 7.85 MPa
>= 1140 psi
ASTM D 638
Elongation at Break >= 300 %
>= 300 %
ASTM D 638
Component Elements Properties Metric English Comments
Cadmium, Cd <= 0.0050 %
<= 0.0050 %
IEC 62321
Chromium, Cr <= 0.010 %
<= 0.010 %
IEC 62321
Lead, Pb <= 0.010 %
<= 0.010 %
IEC 62321
Mercury, Hg <= 0.010 %
<= 0.010 %
IEC 62321
Descriptive Properties Value Comments
Application Automotive
Bromine, Br (%) < 0.01
IEC 62321