Karina 6148/1-RTR Kariprene Black

Category Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 6148/1-RTR Kariprene Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Density 0.900 - 0.960 g/cc
0.0325 - 0.0347 lb/in³
ASTM D 792
ASTM Color -0.970 - -0.170
-0.970 - -0.170
Color B, ME 12
-0.840 - -0.040
-0.840 - -0.040
Color A, ME 12
55.7 - 56.5
55.7 - 56.5
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 58 - 62

@Time 15.0 sec
58 - 62

@Time 0.00417 hour
ASTM D 2240
62

@Time 15.0 sec
62

@Time 0.00417 hour
After Injection Molding; ASTM D 2240
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Elongation at Break >= 450 %
>= 450 %
ASTM D 638
Abrasion <= 220
<= 220
mm<sup>3</sup>; DIN 53516
Descriptive Properties Value Comments
Application General Purpose Soles